Lateral Force Microscopy (LFM)
While more traditional AFM techniques focus on vertical deflections of the cantilever to image the surface topography, lateral force microscopy (LFM) instead focuses on torsional deflections as the cantilever scans across the surface. The amount the cantilever twists as the tip is dragged across a sample surface provides useful insight into the frictional force and adhesion properties of the sample.